ตัวกรองผลการค้นหา
Blue Vitriol Copper sulfate
แปลว่า(english) A layout solution which turns a copper color when applied to a clean,polished metal surface.
Bruise
แปลว่า(english) A mark transferred to the strip surface from a defective process roll. Similar to dent or punchmark.
Bright Annealing
แปลว่า(english) A process carried out usually in a controlled furnace atmosphere, so surface does not oxidize, remaining bright.
Activation
แปลว่า(english) The changing of the passive surface of a metal to a chemically active state. Contrast with passivation.
External force:
แปลว่า(english) A surface force or body force acting on an object. External forces are sometimes called applied forces.
Peeling
แปลว่า(Concrete Engineering) A process in which thin flakes of matrix or mortar are broken away from concrete surface; caused by adherence of surface mortar-to forms as forms are removed, or to trowel or float in portland cement plaster.
Pining
แปลว่า(Concrete Engineering) Development of relatively small cavities in a concrete surface, due to phenomena such as cavitation or corrosion.
Bright Annealing 2
แปลว่า(english) The process of annealing in a protective atmosphere so as to prevent discoloration of the bright surface desired.
Bonderized Coating
แปลว่า(english) A thin film of phosphate pretreatment applied to a steel surface (bare or zinc coated) to enhance paintability.
Bright Dipping
แปลว่า(english) Chemical polishing of aluminum, often by treatment with a mixture of nitric acid and phosphoric acid, yielding a mirror-shiny (specular) highly reflective surface. It is almost always followed by anodizing to protect the surface and provide some choice of color.
Brite
แปลว่า(english) 1) Regular galvanize coating (not minimized spangle or JP). 2) Rolls that have no grit; smooth finish on surface of steel.
Burnt Rubber